Polymer Property : Tensile Strength, Yield = 0.117 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.117 MPa
17.0 psi
ASTM D-412 (Die A)
Saint-Gobain Norton® V770 Low-Density Pressure Sensitive Adhesive Sealant Foam
Description: Low Density Foam Suitable for Sealing of Thin Gauge Metals and Plastics. Closed cell polyvinyl chloride foam sealant with pressure sensitive adhesive on one side. The tight bonding adhe..
Tensile Strength, Yield 0.117 MPa
17.0 psi
ASTM D412
ACC Magnifoam™ MF1-9575™ MTI Silicones Silicone Foam
Part of the Amber Chemical Group. Data provided by manufacturer.
Tensile Strength, Yield 0.117 MPa
17.0 psi
Wet; ASTM 686-76
Unifrax Fiberfrax® Moist Pak-D® Ceramic Fiber Insulator
Fiberfrax Moist Pak-D insulation is made from high-strength ceramic fiber blankets impregnated with inorganic bonding agents. This processing results in a flexible insulation that air dries to form..