Mechanical Properties Metric English Comments
Falex Load Test >= 907000 g
>= 2000 lb
ASTM 3233-B
ConocoPhillips ANDEROL® AA-30 White Mineral Food Grade Oil, ISO Grade 68/100, SAE Grade 30
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Falex Load Test >= 907000 g
>= 2000 lb
ASTM 3233-B
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Falex Load Test >= 907000 g
>= 2000 lb
ASTM 3233-B
ConocoPhillips ANDEROL® AA-10 White Mineral Food Grade Oil, ISO Grade 32, SAE Grade 10W
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Falex Load Test >= 907000 g
>= 2000 lb
ASTM 3233-B
ConocoPhillips ANDEROL® AA-20 White Mineral Food Grade Oil, ISO Grade 46, SAE Grade 20
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Falex Load Test 907000 g
2000 lb
ConocoPhillips Hydroclear® 32 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
Falex Load Test 907000 g
2000 lb
ConocoPhillips Hydroclear® 46 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..
Falex Load Test 907000 g
2000 lb
ConocoPhillips Hydroclear® 68 Rock Oil
Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill ..