Material Notes:
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are recommended for use with hydraulic systems, vacuum pumps, compressors, bearings, gears, slides, ways and chains. It also can be used as a wipe down oil. PQ food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. PQ food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.”Information provided by ConocoPhillips.Anderol® is a registered trademark of The Anderol Company.
Physical Properties Metric English Comments
Specific Gravity 0.880 g/cc
0.880 g/cc
60°F; ASTM D-1298
Viscosity Measurement 105
105
Viscosity Index; ASTM D-2270
Saybolt Viscosity at 100°F 392 SUS
392 SUS
ASTM D-2161
Saybolt Viscosity at 210°F 59 SUS
59 SUS
ASTM D-2161
Kinematic Viscosity at 40°C (104°F) 87 cSt
87 cSt
ASTM D-445
Kinematic Viscosity at 100°C (212°F) 10.6 cSt
10.6 cSt
ASTM D-445
ASTM Color 1.0
1.0
ASTM D-1500
Mechanical Properties Metric English Comments
Four Ball Wear 0.380 mm
0.0150 in
1 hr. @ 1200 rpm, 75°C (167°F), 40 kg.; ASTM 4172
Falex Load Test >= 907000 g
>= 2000 lb
ASTM 3233-B
Timken Test 18100 g
40.0 lb
ASTM D-2782
Thermal Properties Metric English Comments
Pour Point -20.0 °C
-4.00 °F
ASTM D-97
Flash Point 225 °C
437 °F
ASTM D-92
Descriptive Properties Value Comments
Copper Corrosion 1B
3 hrs. at 100°C, ASTM D130
Rust Test Pass
ASTM D665B
Vickers Vane Pump Test Pass
ASTM D2882