Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
NOVA Chemicals Sclair® FP112-A Octene VLDPE Film Resin Features: Low seal initiation temperatureHigh toughnessVery good optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Low gel Applications: Sealant and lamination film for food packagi.. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
NOVA Chemicals Surpass® HPs900-C Octene sLLDPE Film Resin Features: Easy processabilityExceptional clarity and glossLow gelExcellent seal properties Applications: High clarity applications Lamination film Coextruded sealant layerHigh toughness filmInformat.. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1051 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1051 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstandin.. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and .. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D 882 |
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatu.. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
Braskem HM 150 HDPE Monofilament Polyethylene
(discontinued **) Applications: Raschel; flat yarn; general and industrial rape netting. Information provided by Braskem |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | Ultimate; ASTM D882 |
LG Chemical SEETEC ST308 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Excellent puncture resistance, tear strength. Excellent sealing and optical properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplica.. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
Eastman Embrace LV Copolyester for Shrink Film Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo.. |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | ASTM D882 |
Eastman Sahara Film Sahara Films are developed for use in applications where increased temperature resistance is desired.Applications/UsesHigh temperature printable films |
|||
Film Tensile Strength at Break, MD | 49.0 MPa | 7110 psi | |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |