Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
SABIC 118 Series Linear Low Density Polyethylene for Blown Film Product Description: 118 series resins are Linear Low Density Polyethylene grades suitable for general purpose packaging. Films produced using these resins yield good tensile properties, impact st.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-D Hexene LLDPE Film Resin Film Properties. Features: Exceptional toughness, high strength with thin films.Applications: Thin films, premium trash bags, ice bags.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-F Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, low gel count.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
Huntsman Rexell® V8801 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
ExxonMobil Escorene® LD-333 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 9.0% vinyl acetate copolymer film resin. Film made from LD-333 exhibits superior impact strength, clarity and heat sealability.Applications: Prim.. |
|||
Film Tensile Strength at Break, MD | 37.0 - 317 MPa | 5370 - 46000 psi | Average value: 96.7 MPa Grade Count:16 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | Orientation not specified; ASTM D882 |
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882-02 |
Ipiranga Petrochem LB 0316 LLDP IPQ produces Linear Low Density Polyethylene (LLDPE) for use by plastics molding industry segments that employ extrusion processes in the manufacturing of films destined for producing bobbins and ba.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D-882 |
Bapolene® 142A Polyethylene Film Grade Bapolene 142A is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D-882 |
Bapolene® 142B Polyethylene Film Grade Bapolene 142B is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D-882 |
Bapolene® 142F Polyethylene Film Grade Bapolene 142F is a hexene linear low density polyethylene for blown film applications requiring superior impact strength. Product is designed to exhibit performance similar to that of super hexene p.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
Huntsman Rexell® V8403 Cast Film Extrusion LLDPE
(discontinued **) Linear-low very low density copolymer, blown film extrusion, FDA compliantFeatures: Excellent resistance to impact, puncturing, tearing, and flex cracking with good weld seal strength, hot tack, and.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
Film Tensile Strength at Break, MD | 37.0 MPa | 5370 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0119-FP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: High strength and toughness, low gel count, intended for narrow die gaps.Applications: Stretch wrap, blend resin.Data provided by the manufacturer. |