Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 24.9 MPa
3610 psi
ASTM D882
ExxonMobil LD 105.30 Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Film Tensile Strength at Break, MD 24.9 MPa
3610 psi
ASTM D882
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..