Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 23.7 MPa | 3440 psi | ASTM D882 |
Eastman Eastman AP005 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Film Tensile Strength at Break, MD | 23.7 MPa | 3440 psi | ASTM D882 |
ExxonMobil LD 144.50 Packaging Film Resin Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and .. |