Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 814 Polyester Film, 48 Gauge Mylar® 814 is a one-side pretreated polyester film which was designed for UV cure inks and also works well for EB cure overlaquers. General Product Info: Mylar® 814 is designed to provide excellen.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 823 Polyester Film, 48 Gauge Mylar® 823 is a two side, differentially pretreated, polyester film designed to provide excellent adhesion in print and lamination applications.Approvals: FDA Food Contact Status - All gauges of My.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 65 Gauge (17 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 80 Gauge (20 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882A |
DuPont Teijin Films Mylar® X842 Polyester Film, 48 Gauge Mylar® X842 is a clear polyester film that has been chemically treated on both sides for the packaging converting market. One side is chemically treated for metal adhesion. The other side is chemic.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 822 Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Melinex® 822 is a polyester film that has been chemically pretreated on one side. It is designed for printing and extruded polyethylene adhesion. Melinex.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882 |
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882A |
DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge Mylar® M813 is a clear, pretreated base film with high gloss, low haze, and excellent processability. It is a one side pre-treated polyester designed for improved ink adhesion and may be suitable f.. |
|||
Film Tensile Strength at Break, MD | 214 MPa | 31000 psi | ASTM D882A |
DuPont Teijin Films Mylar® 864 Polyester Packaging Film, 48 Gauge Data provided by DuPont Packaging Polymers.Melinex® 864 is a polyester film, chemically treated on two sides. Both sides are designed for printing and extruded polyethylene adhesion. One side is en.. |