Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 89.5 MPa | 13000 psi | Calculated from mfr's report of 291 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Film Tensile Strength at Break, MD | >= 89.6 MPa | >= 13000 psi | ASTM D882 |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Film Tensile Strength at Break, MD | >= 89.6 MPa | >= 13000 psi | ASTM D882 |
DuPont™ Tedlar® TUT10BG3 UV Screening Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Film Tensile Strength at Break, MD | 89.6 MPa | 13000 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 70LS447 OPP Film Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print su.. |
|||
Film Tensile Strength at Break, MD | 89.6 MPa | 13000 psi | ASTM D882 |
Dow SARAN WRAP™ 3 Plastic Film SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls.. |
|||
Film Tensile Strength at Break, MD | 89.6 MPa | 13000 psi | ASTM D882 |
ExxonMobil Exceed™ 3518CB Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 3518CB is a metallocene ethylene-hexene copolymer. Films made of Exceed 3518CB grade have outstanding tensile, impact and puncture resistance properties. Furthermore, the.. |