Polymer Property : Film Tensile Strength at Break, MD = 95.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 95.0 MPa
13800 psi
UBE 1022FDX29 Nylon 6 Homopolymer Film
Specialties: Nucleated (Medium viscosity) Processing: T-die, Air blown Applications: General applications Information provided by UBE.
Film Tensile Strength at Break, MD 95.0 MPa
13800 psi
ASTM D882
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness...
Film Tensile Strength at Break, MD 95.0 MPa
13800 psi
ASTM D882
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness...