Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 90.3 MPa | 13100 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Metallyte™ 28MWHB OPP Film Product Description: A multi-layer, cavitaed, white OPP film that has exceptional barrier to gases, flavors and moistures. It is metalized on one side with a proprietary sealant layer on the other. .. |
|||
Film Tensile Strength at Break, MD | 90.3 MPa | 13100 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 150LL-302 OPP Film Product Description: A white, corona-treated polypropylene label facestock designed for rigid and semi-rigid pressure-sensitive applications requiring durability, opacity, and excellent graphic appe.. |