Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 310 - 379 MPa | 45000 - 55000 psi | ASTM D882 |
Honeywell Capran® Unidraw (0.75 mil) Nylon 6 Film
(discontinued **) Description: Capran® Unidraw is a 0.75 mil (19 micron) machine direction oriented nylon 6 film specifically designed for the continuous process lamination of glass fiber reinforced panel. High str.. |
|||
Film Tensile Strength at Break, MD | 310 MPa | 45000 psi | ASTM Data |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Film Tensile Strength at Break, MD | 310 MPa | 45000 psi | Orientation not specified; ASTM D882 |
DuPont™ Kapton® 100EN Polyimide Film, 25 Micron Thickness Film thickness 25 micron (1.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications req.. |
|||
Film Tensile Strength at Break, MD | 310 MPa | 45000 psi | Orientation not specified; ASTM D882 |
DuPont™ Kapton® 200EN Polyimide Film, 50 Micron Thickness Film thickness 50 micron 2.0 mil)Kapton® Type E and EN films have superior dimensional stability, low CHE, a CTE close to copper, and a high modulus. This type is exceptional for applications requ.. |