Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345013 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene ApplicationsPETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optic.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM-D882 |
Westlake EB502 12.5% EVA Copolymer Westlake Elevate™ EB502 resin is a fractional melt index 12.5% VA ethylene vinyl acetate copolymer designed for flexible packaging and other films that require excellent toughness and good heat sea.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D638 |
Westlake Elevate™ EF598 9% Ethylene Vinyl Acetate Copolymer Westlake EF437 resin is a 2.5% EVA copolymer designed for films that require excellent optical and strength properties. This Kosher compliant resin has excellent heat sealing characteristics and low.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D638 |
Westlake EMAC® EF598AA 9% Ethylene-Methyl Acrylate Copolymer Clarity optics, excellent drawdown, excellent machinability, good TD heat shrinkage and excellent toughness. Uses include food packaging tie layers, heat seal layers, extrusion coating, cast film, .. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | ASTM D882 |
Westlake LF1040 Butene Linear Low Density Polyethylene Westlake LF1040 is a butene LLDPE resin with excellent mechanical and sealing properties. It can be used in stretch film and can liner applications, and is suitable for blending with LDPE in packagi.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | Non-oriented film; ASTM D882 |
Total PPR 7450HC Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its .. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Film Tensile Strength at Break, MD | 27.6 MPa | 4000 psi | |
Dow LDPE 683I Low Density Polyethylene, Film Grade DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.. |