Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
LyondellBasell Petrothene® NA952000 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
LyondellBasell Petrothene® NA952094 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
LyondellBasell Petrothene® NA480145 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3210 psi | D638 |
Westlake EF524 14.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF524 is an ethylene vinyl acetate copolymer with 14.5% VA. EF524 is designed for blown and
cast films requiring excellent optics and low heat seal initiation. High melt strength.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 368HD Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 368ON Low Density Polyethylene Resin Product Description: LD 368 series are high clarity EVA LDPE grades, offering good optical properties combined with toughness and impact resistance. Two additive combinations are available according.. |
|||
Film Tensile Strength at Break, MD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |