Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength MD | 510 g | 510 g | ISO 6383-2 |
EMS-Grivory Grivory® HB 5299 HV PA* Product description: Grivory HB 5299 HV is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. HV indicates high viscosity, sui.. |
|||
Elmendorf Tear Strength MD | 510 g | 510 g | ISO 6383-2 |
EMS-Grivory Grivory® HB5299 PA* Product description: Grivory HB 5299 is a lubricated, lactam free copolyamide, especially developed for high barrier (oxygen, carbon dioxide) packaging solutions. Excellent oxygen and carbon dioxide.. |
|||
Elmendorf Tear Strength MD | 510 g | 510 g | ASTM D1922 |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
Elmendorf Tear Strength MD | 510 g | 510 g | ASTM D1922 |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Elmendorf Tear Strength MD | 510 g | 510 g | ASTM D1922 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Elmendorf Tear Strength MD | 510 g | 510 g | ASTM D1922 |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Elmendorf Tear Strength MD | 510 g | 510 g | ASTM D1922 |
Huntsman Rexell® V8401 Cast Film Extrusion LLDPE
(discontinued **) Ultra linear-low density copolymer, blown film extrusion, FDA compliant.Features: Excellent combination of flexibility, flex crack resistance, and low temperature properties. It also exhibits excell.. |