Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.59 GPa | 521 ksi | Tensile 0.5% Secant Modulus; ASTM D638 |
Greene Tweed Arlon® 1330 PEEK Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |