Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
ASTM D882
Eastman 1830F Polyethylene  (discontinued **)
Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and..
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
ASTM D882
Eastman E6838-922F Polyethylene  (discontinued **)
E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat..
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
ISO 527-3
Total HDPE HL 717 High Density Polyethylene - Blown Film
HDPE HL 717 is a high density polyethylene produced by the gas phase polymerization process with hexene as a comonomer.HDPE HL 717 is a monomodal HDPE with a broad molecular weight distribution. It..
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
parallel; ISO 527-3
DSM Akulon® F130-E1 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
parallel; ISO 527-3
DSM Akulon® F130-E5 PA6
Medium Viscosity, Nucleated, Lubricated, Film Extrusion, Antiblock
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
parallel; ISO 527-3
DSM Akulon® F132-E1 PA6
Medium/High Viscosity, Nucleated, Lubricated, Film Extrusion
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
parallel; ISO 527-3
DSM Akulon® F132-E2 PA6
High Viscosity, Nucleated, Lubricated, Film Extrusion
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
parallel; ISO 527-3
DSM Akulon® F136-E1 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion
Film Tensile Strength at Yield, MD 34.0 MPa
4930 psi
parallel; ISO 527-3
DSM Akulon® F136-E2 PA6
Very High Viscosity, Lubricated, Nucleated, Film Extrusion