Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 15.2 MPa | 2200 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-C Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Film Tensile Strength at Yield, MD | 15.2 MPa | 2200 psi | ASTM D882 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Film Tensile Strength at Yield, MD | 15.2 MPa | 2200 psi | ASTM D882 |
ExxonMobil LLDPE LL 3402.48 Cast Linear Low Density Polyethylene Resin Product Description: LL 3402.48 is a hexane medium density polyethylene cast film grade for applications requiring high stiffness. It can also be used in blown films. Films produced from this resin .. |
|||
Film Tensile Strength at Yield, MD | 15.2 MPa | 2200 psi | |
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2037 Polyethylene is a cast film extrusion resin for high stiffness film applications. It complies with U.S. FDA regulation 21 CFR 177.1520 c 3.2a when used unmodified and according to good.. |
|||
Film Tensile Strength at Yield, MD | 15.2 MPa | 2200 psi | |
Dow LDPE 768A Low Density Polyethylene, Film Grade DOW LDPE 768A resin is a medium density film resin with additional stabilization for films requiring high modulus such as paper overwrap. It contains low levels of both slip additive and antiblock a.. |
|||
Film Tensile Strength at Yield, MD | 15.2 MPa | 2200 psi | ASTM D882 |
Bapolene® 200F Polyethylene, Film Grade Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets FDA standards for foo.. |