Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow DOWLEX™ 2045.02AC Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2045.02AC Polyethylene resin is a high stability blown film extrusion resin that provides excellent tear strength and outstanding toughness. It contains high level of slip additive and medi.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow Elite® 5200 Linear Low Density Polyethylene 5200 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. This resin offers high impact strength and good puncture resistance at moderate stretch levels for .. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 133A Low Density Polyethylene, Blown Film Grade DOW LDPE 133A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of antib.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 135A Low Density Polyethylene, Blown Film Grade DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip .. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 503A Low Density Polyethylene, Liner Film Grade DOW LDPE 503A resin is used for liner film and other packaging applications that require optical clarity. It contains medium levels of slip additive and low levels of antiblock additive. It complies.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 682I Low Density Polyethylene, Film Grade DOW LDPE 682I barefoot resin is used for shrink, frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food contact applications. T.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 683I Low Density Polyethylene, Film Grade DOW LDPE 683I resin is a general purpose resin with low levels of antiblock additive used for frozen food, and heavy duty film applications. This material complies with U.S.FDA regulation 21 CFR 177.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | |
Dow LDPE 132I Low Density Polyethylene, Blown Film Grade DOW LDPE 132I is a barefoot resin for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It complies with U.S. FDA re.. |
|||
Film Tensile Strength at Yield, MD | 10.3 MPa | 1490 psi | ASTM D-882 |
Bapolene® 122B Polyethylene, Film Grade Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets .. |