Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow LDPE 135A Low Density Polyethylene, Blown Film Grade

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow LDPE 135A Low Density Polyethylene, Blown Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DOW LDPE 135A resin is used for heavy duty blown film applications such as shrink film, shipping sacks, construction film, and other thick gauge film applications. It contains medium levels of slip and antiblock additives. It complies with U.S. FDA regulation 21 CFR c 2.1 for food contact applications. The regulation should be consulted for complete details.Film properties below based on a film thickness of 76 µm. Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
Thickness 76.0 microns
2.99 mil
Melt Flow 0.22 g/10 min

@Load 2.16 kg
0.22 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 10.3 MPa
1490 psi
Film Tensile Strength at Yield, TD 9.70 MPa
1410 psi
Film Elongation at Break, MD 450 %
450 %
Film Elongation at Break, TD 540 %
540 %
Coefficient of Friction 0.10
0.10
Elmendorf Tear Strength MD 290 g
290 g
Elmendorf Tear Strength TD 380 g
380 g
Elmendorf Tear Strength, MD 3.80 g/micron
96.5 g/mil
Elmendorf Tear Strength, TD 5.00 g/micron
127 g/mil
Dart Drop 3.90 g/micron
99.1 g/mil
Film Tensile Strength at Break, MD 23.4 MPa
3390 psi
Film Tensile Strength at Break, TD 17.9 MPa
2600 psi
Optical Properties Metric English Comments
Haze 12 %
12 %
Gloss 52 %
52 %
45°
Processing Properties Metric English Comments
Processing Temperature 216 °C
421 °F
Film extrusion temperature