Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.130 MPa-m/sec | 3710 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Limiting Pressure Velocity | 0.130 MPa-m/sec | 3710 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Limiting Pressure Velocity | 0.130 MPa-m/sec | 3710 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Limiting Pressure Velocity | 0.130 MPa-m/sec | 3710 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Limiting Pressure Velocity | 0.130 MPa-m/sec | 3710 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Limiting Pressure Velocity | 0.130 MPa-m/sec | 3710 psi-ft/min | at 0.1 m/s unlubricated |
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |