Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 495 MPa @Diameter 12.7 mm, Temperature 25.0 °C |
71800 psi @Diameter 0.500 in, Temperature 77.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 495 MPa @Strain 0.200 %, Temperature 200 °C |
71800 psi @Strain 0.200 %, Temperature 392 °F |
Bar |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 495 MPa @Strain 0.200 %, Thickness 7.90 - 25.0 mm |
71800 psi @Strain 0.200 %, Thickness 0.311 - 0.984 in |
Typical Strength |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | 495 MPa @Strain 0.200 %, Thickness 25.0 - 100 mm |
71800 psi @Strain 0.200 %, Thickness 0.984 - 3.94 in |
Typical Strength |
Constellium Certal® Thick Aluminum Plate Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and .. |
|||
Tensile Strength, Yield | >= 495 MPa @Strain 0.200 % |
>= 71800 psi @Strain 0.200 % |
Minimum |
Aleris Hokotol Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |