Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 373 MPa @Temperature 20.0 °C |
>= 54100 psi @Temperature 68.0 °F |
Condition T6 (Quenching in water at 80C) |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 373 MPa @Strain 0.200 %, Thickness 12.7 mm |
54100 psi @Strain 0.200 %, Thickness 0.500 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |