Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2720 MPa @Temperature 25.0 °C |
395000 psi @Temperature 77.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |