Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 2090A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 23.0 MPa

@Strain 300 %
3340 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 1090A Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products ..
Tensile Strength, Yield 23.0 MPa

@Temperature 871 °C
3340 psi

@Temperature 1600 °F
ATI Allegheny Ludlum AL 453™ Stainless Steel
Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum
Tensile Strength, Yield 23.0 MPa

@Strain 10.0 %
3340 psi

@Strain 10.0 %
ASTM D638
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang.