Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 216 MPa @Temperature 23.0 °C |
31300 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |
|||
Tensile Strength, Yield | 216 MPa @Strain 0.200 %, Temperature 427 °C |
31300 psi @Strain 0.200 %, Temperature 801 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |