Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 174 MPa @Temperature -55.0 °C |
25300 psi @Temperature -67.0 °F |
90°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber Information provided by HexCel |