Polymer Property : Tensile Strength, Yield = 2130 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.7 MPa

@Strain 300 %
2130 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 185A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 14.7 MPa

@Strain 5.00 %
2130 psi

@Strain 5.00 %
ASTM D638
SK Chemicals SKYPEL G168D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 14.7 MPa

@Strain 300 %
2130 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 585A X series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 14.7 MPa

@Strain 50.0 %
2130 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 14.7 MPa

@Strain 50.0 %
2130 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 14.7 MPa

@Strain 10.0 %
2130 psi

@Strain 10.0 %
ASTM D638
Samyang Triel® 5550 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5550 is an extrusion grade.Information provided by Samyang.