Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 965 MPa @Strain 1.00 % |
140000 psi @Strain 1.00 % |
ASTM E345-93, Type A Specimen |
NiCoForm NiColoy® E Electroformed Nickel-Cobalt NiColoy® is a proprietary electrodeposited Nickel-Cobalt alloy distinguished by the following combination of features:Leveled, smooth matte to semi bright deposit with low internal stressHigh tensi.. |
|||
Tensile Strength, Yield | >= 965 MPa @Strain 0.200 % |
>= 140000 psi @Strain 0.200 % |
|
PSM Industries PolyAlloys MIM-14-4PH Heat Treated Stainless Steel PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of compl.. |
|||
Tensile Strength, Yield | 963 MPa @Strain 0.200 %, Thickness 3.20 mm |
140000 psi @Strain 0.200 %, Thickness 0.126 in |
30% cold reduction |
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 %, Temperature 371 °C |
140000 psi @Strain 0.200 %, Temperature 700 °F |
843°C Hardening Temp |
Latrobe CBS-600™ VIM-VAR Carburizing Bearing and Gear Steel CBS-600 VIM-VAR is a carburizing bearing and gear steel designed for service temperatures up to 600°F. Double vacuum melting is employed to provide optimum tensile properties as well as describe.. |
|||
Tensile Strength, Yield | 965 MPa @Temperature 752 °C |
140000 psi @Temperature 1390 °F |
|
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica.. |
|||
Tensile Strength, Yield | 965 MPa @Temperature -55.0 °C |
140000 psi @Temperature -67.0 °F |
0°, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 963 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
Longitudinal |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
Cold-Worked Full hard |
AK Steel 201 Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
Cold-Worked Full hard |
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Tensile Strength, Yield | 965 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
Cold-Worked Full hard |
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Tensile Strength, Yield | 967 MPa @Strain 0.200 % |
140000 psi @Strain 0.200 % |
Longitudinal |
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 1150 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |