Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 95.0 MPa @Temperature 20.0 °C |
>= 13800 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S220 Aluminum Alloy, AlSi35, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 95.0 MPa @Temperature 200 °C |
13800 psi @Temperature 392 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |