Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.998 MPa

@Temperature 22.2 °C
1305 psi

@Temperature 72.0 °F
Flatwise Tensile, Primed with Redux 119
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf)
Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve..
Tensile Strength, Yield 8.998 MPa

@Temperature 21.1 °C
1305 psi

@Temperature 70.0 °F
Flatwise Tension
Hexcel® Redux® 322U Modified epoxy film adhesive (0.06 psf)
Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up ..
Tensile Strength, Yield 8.998 MPa

@Temperature 149 °C
1305 psi

@Temperature 300 °F
Flatwise Tensile
Hexcel® Redux® 641K Modified epoxy film adhesive for bonding metallic and composite components
Redux 641 is a high temperature modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures where operating temperatures are experienced up t..