Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Tensile Strength, Yield | 78.5 MPa @Thickness 3.20 mm |
11400 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |