Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 785 MPa @Strain 0.200 %, Temperature 760 °C |
114000 psi @Strain 0.200 %, Temperature 1400 °F |
|
Haynes R-41 alloy, 0.635 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, aged 16 hours at 760°C (1400°F), air cooled Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ.. |
|||
Tensile Strength, Yield | 785 MPa @Treatment Temp. 593 °C, Time 1.44e+7 sec |
114000 psi @Treatment Temp. 1100 °F, Time 4000 hour |
0.2%. Room temp test after thermal exposure |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 785 MPa @Strain 0.200 % |
114000 psi @Strain 0.200 % |
15.1% Cold Work |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |