Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 53.0 MPa @Temperature 23.0 °C |
7690 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 157HSL BK010 Nylon 612
(Unverified Data**) Zytel® 157HSL BK010 is a heat stabilized, weatherable, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |