Polymer Property : Tensile Strength, Yield = 5.70 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.70 MPa

@Strain 100 %
827 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 1185A Poly(adipate)ester TPU Resin
ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp..
Tensile Strength, Yield 5.70 MPa

@Strain 100 %
827 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..