Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 202 MPa @Temperature 177 °C |
29300 psi @Temperature 351 °F |
T300 (6K); [+/- 45°]2s |
Hexcel® HexPly® F655 Bismaleimide Resin, Carbon Tape Form Fiber: T300-12K, IM7-12KInformation provided by HexCel |