Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 20.0 MPa @Temperature 23.0 °C |
2900 psi @Temperature 73.4 °F |
90° |
Hexcel® HexPly® 954-3 Curing Cyanate Resin, K13C-2U Fiber Information provided by HexCel |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 65.0 °C |
2900 psi @Temperature 149 °F |
ASTM D638 |
BASF Ultramid® 8281 HS GP PA6 (Dry) Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p.. |
|||
Tensile Strength, Yield | 20.0 MPa @Strain 100 % |
2900 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1154D Polyether Type Polyurethane Elastomer Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exh.. |
|||
Tensile Strength, Yield | 20.0 MPa @Strain 300 % |
2900 psi @Strain 300 % |
ASTM D-412 |
BASF Elastollan® S90A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue.. |
|||
Tensile Strength, Yield | 20.0 MPa @Strain 100 % |
2900 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PB581-H Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |