Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1772 MPa @Temperature 93.0 °C |
257000 psi @Temperature 199 °F |
Dry |
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |