Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 170 MPa @Strain 1.00 %, Temperature 600 °C |
24700 psi @Strain 1.00 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 300 °C |
24700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 300 °C |
24700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 300 °C |
24700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 1093 °C |
24700 psi @Strain 0.200 %, Temperature 1999 °F |
Longitudinal |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
|
Crucible Compaction Metals Rene Supersolvus Rene 95 Nickel Based Superalloy Supersolvus P/M Rene 95 is designed to provide even higher temperature creep resistance and stress rupture strength than subsolvus Rene 95. Chemistry is not modified. These properties are obtained.. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 649 °C |
24700 psi @Temperature 1200 °F |
ASTM E8 |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |