Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.7 MPa @Strain 300 % |
2130 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 185A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 14.7 MPa @Strain 5.00 % |
2130 psi @Strain 5.00 % |
ASTM D638 |
SK Chemicals SKYPEL G168D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Tensile Strength, Yield | 14.7 MPa @Strain 300 % |
2130 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 585A X series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 14.7 MPa @Strain 50.0 % |
2130 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM460 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 14.7 MPa @Strain 50.0 % |
2130 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® PM460 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Tensile Strength, Yield | 14.7 MPa @Strain 10.0 % |
2130 psi @Strain 10.0 % |
ASTM D638 |
Samyang Triel® 5550 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5550 is an extrusion grade.Information provided by Samyang. |