Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 10.0 - 5040 x 10-8 mm³/N-M | 4.96 - 2500 x 10-10 in³-min/ft-lb-hr | Average value: 4080 x 10<sup>-8</sup> mm³/N-M Grade Count:18 |
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum.. |
|||
K (wear) Factor | 10.0 - 142 x 10-8 mm³/N-M | 4.96 - 70.6 x 10-10 in³-min/ft-lb-hr | Average value: 39.6 x 10<sup>-8</sup> mm³/N-M Grade Count:8 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
K (wear) Factor | 10.0 - 20.0 x 10-8 mm³/N-M | 4.96 - 9.93 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon® |
|||
K (wear) Factor | 10.0 - 15.0 x 10-8 mm³/N-M | 4.96 - 7.45 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon® |
|||
K (wear) Factor | 10.0 - 15.0 x 10-8 mm³/N-M | 4.96 - 7.45 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G405 Polytetrafluoroethylene 25% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
K (wear) Factor | 10.0 x 10-8 mm³/N-M | 4.96 x 10-10 in³-min/ft-lb-hr | |
LATI Latilub 80-10T G/40 PPS, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
K (wear) Factor | 10.0 - 100 x 10-8 mm³/N-M | 4.96 - 49.6 x 10-10 in³-min/ft-lb-hr | |
BACT Dylyn® Diamond-Like Nanocomposite Coating a-C:H/a-Si:O nanocomposite. This coating provides the lowest friction of the BACT products, even in high humidity or wet environments. It offers an excellent combination of anti-stick and wear be.. |
|||
K (wear) Factor | 10.0 - 100 x 10-8 mm³/N-M | 4.96 - 49.6 x 10-10 in³-min/ft-lb-hr | |
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating Metal-doped Me/a-C:H/a-Si:O nanocomposite. The electrical characteristics of these coatings can be tailored by the addition of metal dopants. This creates an engineered surface for specialized ap.. |
|||
K (wear) Factor | 10.0 - 20.0 x 10-8 mm³/N-M | 4.96 - 9.93 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |
|||
K (wear) Factor | >= 10.0 x 10-8 mm³/N-M | >= 4.96 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |