Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 32.0 x 10-8 mm³/N-M | 15.9 x 10-10 in³-min/ft-lb-hr | at 5000 psi - fpm PV; ASTM D3702 |
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled
(discontinued **) Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon. |