Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1370 MPa | 198000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP8255E1 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for compounded and injection molded applications requiring high melt flow rate and excellent processing attributes... |