Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM D790A
SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding
Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent i..
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM D 790
NOVA Chemicals Sclair® IG464-C Injection Molded HDPE Resin
IG464-C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG464..
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Braskem H 125 HOMO Polypropylene Homopolymer
H 125 is a high melt flow rate homopolymer designed for nonwoven by spunbonded processing. It is used in fiber extrusion processing. This resin features excellent processing, allowing increased line..
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Braskem H 214 HOMO Polypropylene Homopolymer
H 214 is a high melt flow rate homopolymer with narrow molecular weight distribution. It is specially designed for fiber extrusion and nonwoven applications. This product presents excellent processa..
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM D790A
Braskem H 603 Extrusion Polypropylene Homopolymer
Flat and corrugated sheets in general.Information provided by Braskem.
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Braskem PH 0130 HOMO Polypropylene Homopolymer
PH 0130 is a low melt flow rate homopolymer with a general purpose additive package. This resin is designed for blow molding and extrusion. PH 0130 features excellent processability and stiffness/im..
Flexural Modulus, 1% Secant 1300 MPa
189000 psi
ASTM-D790
Braskem IA59 HDPE Injection Molding Polyethylene Homopolymer
IA59 is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for injection molding applications. It offers high processability and low warpage and contai..