Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1000 MPa
145000 psi
ASTM-D790
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Prisma 3410 is a medium melt flow rate random copolymer designed for injection molding. This product exhibits exceptional transparency, very good stiffness/impact strength balance, and excellent pro..
Flexural Modulus, 1% Secant 1000 MPa
145000 psi
1% secant; ASTM D790A
Braskem CP 286 Injection Molding Polypropylene Heterophasic Copolymer
Description: CP 286 is a high melt flow rate, heterophasic copolymer, suitable for injection moulding applications and also as base resin for compound. The resin combines excellent stiffness with g..
Flexural Modulus, 1% Secant 1000 MPa
145000 psi
ASTM-D790
Braskem CP 743 HECO Polypropylene Heterophasic Copolymer
CP 743 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and a general purpose additive package. CP 743 presents high melt strength, good processability, and..
Flexural Modulus, 1% Secant 1000 MPa
145000 psi
ASTM-D790
Braskem RP 145 RACO Random Polypropylene Copolymer
RP 145 is a high melt flow rate random copolymer designed for use in thin-walled injection molding parts. This product offers good transparency, very good stiffness/impact strength balance, excellen..