Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 979 MPa @Temperature 23.0 °C |
142000 psi @Temperature 73.4 °F |
0.05 in/min test speed |
Ineos N20L-00 Polypropylene Impact Copolymer This is a nucleated polypropylene impact copolymer formulated with a slip agent for improved mold release, and has an optimum balance of stiffness and impact resistance for injection molding applica.. |