Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 412MK49 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 412MK49 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact r.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 49MK45 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 49MK45 is specially developed for producing injection molded articles. This grade contains an antistatic & nucleating agents. It has medium flow properties, good impact re.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 500P Polypropylene Homopolymer for Raffia Applications Product Description: PP 500P is specially developed for producing stretched tapes with the following features:Consistent processabilityEasy orientationLow water carry overGood mechanical properties.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 506P Polypropylene Homopolymer for Raffia Applications Product Description: PP 506P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speeds and low deniersLow tap.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 519A Polypropylene Homopolymer for Spunbond Applications Product Description: PP 519A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 519A has the following features:Consis.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 521P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 521P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
SABIC PP 523P Polypropylene Homopolymer for Bi-axially Oriented Film Product Description: PP 523P is a non formulated grade, specially developed for bi-axially oriented PP (BOPP) film extrusion with a very specific molecular structure providing ultimate properties r.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 217000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil AP03B Polypropylene Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with high melt flow rate and excellent processing attributes. It is designed for injection molded large appliance applicatio.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
Braskem H 155 Fiber Extrusion Polypropylene Homopolymer Meltblown nonwoven applications for hygienic, medical and hospital disposable devices; Filters and oil adsorbents.Information provided by Braskem. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM-D790 |
Braskem PH 1721 HOMO Polypropylene Homopolymer PH 1721 is a low melt flow rate polypropylene with an anti-gas fading stabilization package. It is suitable for continuous filament and staple fiber processing due to its molecular weight distributi.. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | ASTM D790A |
Braskem CP 405XP Compression Molding Polypropylene Heterophasic Copolymer Bottle caps for carbonated beverages.Information provided by Braskem. |
|||
Flexural Modulus, 1% Secant | 1500 MPa | 218000 psi | 0.05 in/min test speed |
Ineos H19G-00 Polypropylene Homopolymer This is a homopolymer designed for extrusion processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsContinuous Filament YarnBCFSta.. |