Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil AXO3BE3 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt fl.. |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM D790 |
Braskem GF4950 HDPE Blow Molding Polyethylene Copolymer HDPE GF4950 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high environmental stress cracking resistance and processability. It was.. |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM D790 |
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness... |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM-D790 |
Braskem HC7260LS-L HDPE Injection Molding Polyethylene HC7260LS-L is a high-density polyethylene developed for injection molding. It has high hardness and stiffness and low warpage. This resin also has additives against ultraviolet radiation action. Its.. |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM D790 |
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta.. |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM D790A |
Braskem H 604 Thermoforming & Extrusion Polypropylene Homopolymer Transparent packaging for food; Flat and corrugated sheets for school and office folders.Information provided by Braskem. |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM-D790 |
Braskem HA7260 HDPE Injection Molding Polyethylene HA7260 is a high-density polyethylene that was developed for injection molding. It is easy to process and has high productivity, high rigidity and hardness, and a good melt flow. Its narrow molar ma.. |
|||
Flexural Modulus, 1% Secant | 1350 MPa | 196000 psi | ASTM D790 |
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene Description: SHC7260 is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. The minimum biobased content of .. |