Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.1 MPa @Treatment Temp. 100 °C, Time 252000 sec |
2630 psi @Treatment Temp. 212 °F, Time 70.0 hour |
Aged ASTM D #3 Oil |
LG Chemical NBR 3250 High Acrylonitrile Polymer Description: NBR 3250 is a copolymer of butadiene and acrylonitrile manufactured by cold emulsion polymerization technology of Goodyear Tire and Rubber Company, USA. NBR 3250 is a non staining, medi.. |
|||
Tensile Strength at Break | 18.1 MPa @Treatment Temp. 100 °C, Time 259000 sec |
2630 psi @Treatment Temp. 212 °F, Time 72.0 hour |
Aged ASTM D #1 Oil |
LG Chemical NBR 6230 High Acrylonitrile Polymer Description: NBR 6230 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6230 is a non staining, low mooney, and m.. |