Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.8 MPa @Temperature 145 °C, Time 1190 sec |
2580 psi @Temperature 293 °F, Time 0.330 hour |
Cured |
LG Chemical NBR 6230 High Acrylonitrile Polymer Description: NBR 6230 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6230 is a non staining, low mooney, and m.. |